Production. Milling machines and machine castings. Pouring a large mold is a fiery sight. To the left, flames are shooting from an escape hole -- caused by gas generated by the contact of iron with the relatively cool sand, graphite, linseed oil and other ingredients involved in the mold structure. The man at the left is wielding a skimmer to hold back any impurities floating on the surface of the ladle iron

Production. Milling machines and machine castings. Pouring a large mol...

Actual size of negative is C (approximately 4 x 5 inches). Title and other information from caption card. Transfer; United States. Office of War Information. Overseas Picture Division. Washington Division; 1944... More